SS 316L Sheet
1. Standard:ASTM A240,ASME SA240
2. Thickness: 0.3~1200mm or as per your requirements
3. Width: 0~2500mm or as per your requirements
4. Length: 0~12m or as per your requirements
316L UNS S31603 stainless steel is a low-carbon austenitic stainless steel. Due to its excellent corrosion resistance, high temperature performance and processing adaptability, it has become a key material widely used in industrial and civil fields. HT PIPE is a SS 316L Plate supplier with 15+ export experience.
Chemical composition of ss316L sheet
The chemical composition of 316L stainless steel is the basis of its performance. Its core elements include: chromium (16%~18%), nickel (10%~14%), molybdenum (2%~3%), and strictly controlled carbon content ( Less than or equal to 0.03%).
corrosion resistance of stainless steel 316L plate
The addition of molybdenum makes it significantly better than 304 stainless steel in resistance to chlorides, acidic media (such as sulfuric acid, phosphoric acid) and marine environments. In addition, the austenitic crystal structure gives it excellent toughness and remains stable even in low temperature environments.

316L Stainless Steel Plate Specifications
| ASTM A240 / ASME SA240 | |
| 0.3mm – 100mm | |
| 0~12m or as per your requirements | |
| 0~2500mm or as per your requirements | |
| Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA , NO(8) | |
Stainless Steel 316L Plate Physical Properties
| 3) | Specific Heat 0-100 degree (J/kg.K) | ||||||||
| 0-100 degree | 0-315 degree | 0-538 degree | at 100 degree | at 500 degree | |||||
| 316L | 8000 | 193 | 15.9 | 16.2 | 17.5 | 16.3 | 21.5 | 500 | 740 |
in line with hygiene standards, used in storage tanks, conveyor belts and food-grade machinery.
SS 316L Plate Weight Chart
| 2000 x1000 x0.7 | 11.5 | 3000 x1500 x1.5 | 55.3 |
| 2500 x1250 x0.7 | 17.9 | 2000 x1000 x2.0 | 32.7 |
| 2000 x1000 x0.9 | 14.7 | 2500 x1250 x2.0 | 51.2 |
| 2500 x1250 x0.9 | 23 | 3000 x1500 x2.0 | 73.7 |
| 2500 x1250 x1.0 | 25.6 | 2000 x1000 x2.5 | 40.9 |
| 2000 x1000 x1.2 | 19.6 | 2500 x1250 x2.5 | 63.9 |
| 2500 x1250 x1.2 | 30.7 | 3000 x1500 x2.5 | 92.1 |
| 3000 x1500 x1.2 | 44.2 | 2000 x1000 x3.0 | 49.6 |
| 2000 x1000 x1.5 | 24.6 | 2500 x1250 x3.0 | 77.5 |
| 2500 x1250 x1.5 | 38.4 | 3000 x1500 x3.0 | 112 |
Cold processing and forming of UNS S31603 Plate
Welding process Stainless steel S31603 plate
It is recommended to use inert gas shielded welding (TIG/MIG), the welding material needs to match the low carbon characteristics (such as ER316L), and the heat input should be controlled to prevent intergranular corrosion.
Heat treatment of SS 316L sheet
Solution treatment (1010~1150 degree rapid cooling) can eliminate processing stress and restore corrosion resistance, but it is necessary to avoid staying in the 450~850 degree range for a long time.
Tolerance of ss316l plate
| w Less than or equal to 84 [2134] | 84 [2134] < w Less than or equal to 120 [3048] | 120 [3048] < w Less than or equal to 144 [3658] | w > 144 [ 3658] | |
| t < 3/16 [4.76] | 0.055 [1.35] | 0.070 [1.78] | - | - |
| 3/16 [4.76] Less than or equal to t < 3/8 [9.52] | 0.045 [1.14] | 0.050 [1.27] | 0.085 [2.16] | - |
| 3/8 [9.52] Less than or equal to t < 3/4 [19.05] | 0.055 [1.40] | 0.060 [1.52] | 0.085 [2.16] | 0.090 [2.29] |
| 3/4 [19.05] Less than or equal to t < 1 [25.04] | 0.060 [1.52] | 0.065 [1.65] | 0.085 [2.16] | 0.100 [2.54] |
| 1 [25.40] Less than or equal to t < 2 [50.80] | 0.070 [1.78] | 0.075 [1.90] | 0.095[2.41] | 0.115 [2.92] |
| 2 [ 50.80] Less than or equal to t < 3 [76.20] | 0.125 [3.20] | 0.150[3.80] | 0.175 [4.45] | 0.200 [5.08] |
| 3 [76.20] Less than or equal to t < 4 [101.6] | 0.150 [3.81] | 0.160 [4.06] | 0.200 [5.08] | 0.225 [5.72] |
| 4 [101.6] Less than or equal to t < 6 [152.4] | 0.180 [4.75] | 0.200 [5.08] | 0.335 [8.50] | 0.355 [9.02] |
| 6 [152.4] Less than or equal to t < 8 [203.2] | 0.235 [6.00] | 0.255 [6.48] | 0.355 [9.02] | 0.435 [11.0] |
| 8 [203.2] Less than or equal to t < 10 [254.0] | 0.315 [8.00] | 0.335 [8.50] | 0.435 [11.0] | 0.550 [14.0] |
Q: About Stainless steel 316L Plate prices?
A: Prices from ranges $2 - $8 per kilogram, vary depending on size, wall thickness, supplier etc.
A: Delivery time is within 5-21 days
Populære tags: ss 316l sheet, Stainless Steel 316L sheet manufacturers, ss S31603 suppliers
Et par
Super duplex 254Smo -arkNeste
SS310MOLN -plateDu kommer kanskje også til å like
Sende bookingforespørsel